Adjustment Factors for Glulam
Same as Sawn Lumber
- load duration factor CD
- time effect factor λ
- temperature factor Ct
- resistance factor Φ
- format conversion factor KF
Wet Service Factor CM
<16% instead of 19%
Flat-Use Factor Cfu
bending about both directions already tabulated
<12" depth around y-axis
rarely needed
Volume Factor CV
test results related to volume instead of size (depth)